Expert article3 min read6 sections

Knowledge centre · Waterproofing & construction

Why fibre glass reinforced membranes split and how to prevent it

Splits, blisters and lap failures in glass reinforced bitumen membranes: what causes them on site and how specification and workmanship prevent them.

Written by the Nuroil trade desk, Sharjah

Pencil sketch of a membrane roll on a roof
On this page · 6 sections
  1. 01Splitting over cracks and joints
  2. 02Cracking during handling
  3. 03Blisters
  4. 04Weak or open laps
  5. 05Shrinkage and ridging
  6. 06What to check before you buy

When a roof laid with fibre glass reinforced bitumen membrane leaks, the cause is rarely the bitumen itself. Most problems trace back to the low stretch of the glass carrier, to how the sheet was handled before laying, or to how it was installed. Knowing the usual failure patterns makes it easier to prevent them on the next job.

Splitting over cracks and joints

A glass mat breaks at a low elongation, typically a few per cent. If the concrete beneath cracks after the membrane is laid, or if a joint between precast units opens with temperature changes, the movement concentrates in a narrow band of membrane directly above it. The sheet cannot stretch enough and splits in a straight line that mirrors the crack below.

  • Allow slabs and screeds to cure and dry before waterproofing.
  • Treat known cracks and construction joints with a separate strip of reinforced sheet laid loose over the joint, so movement is spread over a wider band.
  • Use a polyester-reinforced cap sheet over the glass base layer where movement is expected.

Cracking during handling

Bitumen compound becomes stiff when cold, and oxidised compounds more so than SBS. Unrolling a cold glass-reinforced sheet, or bending it sharply around an upstand, can crack the coating and sometimes the mat. Rolls stored in direct sun can also stick together or deform, making them hard to unroll cleanly. Store rolls upright, shaded and away from heat, and on cool mornings let them warm before unrolling. The low-temperature flexibility value on the data sheet (tested by bending a sample around a mandrel at set temperatures) shows how cold the sheet can get before this becomes a risk.

Blisters

Blisters form when moisture or air is trapped between the membrane and the substrate and then expands in the heat. Common causes are laying on a damp screed, skipping or rushing the primer, and leaving voids when torching. The glass mat does not cause blisters, but because it does not stretch, a blister in a glass sheet is more likely to crack at its edges when walked on.

  • Check that the substrate is dry and clean before priming.
  • Allow the primer to dry fully before torching.
  • Melt the underside evenly so a small bead of compound flows ahead of the roll.

Weak or open laps

Laps are where most leaks start. Typical faults include too small an overlap, insufficient heat at the lap, sand or film left on the bonding area, and end laps lined up in a straight row. On a two-layer system, laps in the cap sheet should be offset from those in the base layer. Probe every lap with a blunt tool once it has cooled and reseal any that lift.

Shrinkage and ridging

Glass-reinforced sheets are chosen partly because they hold their dimensions well. Where shrinkage or ripples do appear, they are often linked to overheating during torching or to a sheet whose compound was not made to specification. Research on bituminous sheets has found that a large share of total shrinkage can occur during melting in manufacture and laying, so both factory control and torch technique matter.

SymptomLikely causePrevention
Straight split above a jointSubstrate movement beyond carrier stretchJoint strips, polyester cap sheet
Surface cracks after unrollingCold or sharply bent sheetWarm rolls; respect cold-flexibility limit
BlistersTrapped moisture or airDry substrate, dry primer, full bond
Lifting lapsPoor heat, contamination, small overlapsCorrect overlap, clean bonding area, probe laps
RipplesOverheating or off-specification sheetTorch control; check data sheet values

What to check before you buy

Many site failures can be headed off at purchase. Ask for the data sheet values for tensile strength, elongation, low-temperature flexibility, flow resistance at high temperature and dimensional stability, and compare them with the project specification. Ask how rolls will be packed and protected in transit. Nuroil provides a certificate of analysis with every delivery of fibre glass reinforced membrane and can arrange third-party inspection on request; send your requirements via request a quote.

PRODUCTS IN THIS ARTICLE
KEEP READING

More from the Knowledge Centre.

STILL HAVE A QUESTION?

Ask the people who trade it every day.

Our trade managers answer technical and commercial questions about grades, specifications, packing and shipping.

LET’S TALK ABOUT YOUR REQUIREMENTS

Your next shipment starts here.

Request a quote