Expert article3 min read5 sections

Knowledge centre · Waterproofing & construction

The cold bending test on SBS membranes and what the result tells you

How the low-temperature flexibility test on SBS modified membranes works, how to read the declared value and why aged results matter.

Written by the Nuroil trade desk, Sharjah

Rolls of BITUROLL-S SBS waterproofing membrane
On this page · 5 sections
  1. 01How the test is carried out
  2. 02Reading the declared value
  3. 03Why the number matters even in warm regions
  4. 04Pairing it with flow resistance
  5. 05What to ask for when buying

Low-temperature flexibility is the property that sets SBS modified bitumen membranes apart. The styrene-butadiene-styrene polymer forms a rubbery network inside the bitumen, so the sheet stays pliable at temperatures where plain oxidised bitumen would crack. The figure that captures this on a data sheet is the cold bending, or cold flexibility, temperature. This article explains how that number is produced and how to use it when comparing SBS sheets.

How the test is carried out

In Europe the method is EN 1109, which determines the flexibility of bitumen sheets at low temperature. Strips cut from the sheet are conditioned in a cold bath or chamber and then bent over a mandrel of fixed radius. After bending, the surface is examined for cracks. The test can be run in two ways:

  • Pass/fail at a set temperature, to confirm that a product meets a declared minimum.
  • Stepped temperatures, lowering the temperature until cracking appears, to find the limiting cold bending temperature of that sample.

Which face is tested depends on the sheet construction. Where the upper surface carries a non-woven or metal facing, or where the reinforcement sits close to the top, the standard directs testing to the bottom face. In North America, the ASTM material specifications for SBS sheets, such as D6164 for polyester-reinforced products, also include a low-temperature flexibility requirement, with their own test conditions.

Reading the declared value

A data sheet might state cold flexibility as, for example, "no cracks at −15 °C" or "≤ −20 °C". A lower (more negative) figure means the compound remains flexible in colder conditions. When comparing products, check three things:

  1. The standard and method. An EN 1109 value and an ASTM value are not directly interchangeable because mandrel size, conditioning and specimen preparation differ.
  2. Whether the value is new or aged. EN 1109 can also be used after artificial ageing (for example under EN 1296 heat ageing) to show how much flexibility the compound loses over time. A sheet that starts at −20 °C but drops sharply after ageing may perform worse in service than one with a slightly warmer initial figure and better retention.
  3. Which face was tested. Results from the top and bottom faces can differ, especially on cap sheets with mineral surfacing.

Why the number matters even in warm regions

Buyers in hot climates sometimes treat cold flexibility as irrelevant. It is not. The cold bending result is a useful indicator of polymer content and compound quality: a well-modified SBS compound typically declares cold flexibility well below freezing, while a poorly modified sheet struggles to do so. Good low-temperature flexibility also tells you the membrane can tolerate the daily thermal cycling on exposed roofs, where surface temperatures swing widely between afternoon and night, and the movement at joints and upstands that comes with it.

It is also relevant during installation. Rolls delivered in cool weather, or stored in air-conditioned warehouses, must be unrolled without cracking. Sheets with poor low-temperature flexibility are more prone to surface crazing when unrolled cold.

Pairing it with flow resistance

Cold flexibility should always be read alongside flow resistance at elevated temperature (EN 1110). The two values define the working window of the compound. SBS compounds generally excel at the cold end, while their resistance to flow at high temperature is usually lower than that of APP compounds. For a roof that sees both cold nights and intense sun, a balanced window matters more than an extreme value at one end.

Ask for cold flexibility before and after ageing. The retained value says more about long-term performance than the initial one.

What to ask for when buying

When you enquire for SBS membranes, ask the supplier to state the cold flexibility value with its test method, the face tested and the result after ageing, alongside flow resistance, reinforcement type and thickness. Request the product data sheet and, where the sheet is sold under EN 13707, the declaration of performance. Nuroil provides a certificate of analysis with every delivery and can arrange third-party inspection on request. Use our quote request form to send the specification you need.

PRODUCTS IN THIS ARTICLE
KEEP READING

More from the knowledge centre.

STILL HAVE A QUESTION?

Ask the people who trade it every day.