Blisters, pinholes and wash-off in SBS bitumen coatings: causes and fixes

Common defects in liquid-applied elastomeric SBS bitumen coatings, what causes each one on site, and how to prevent or repair it.

Written by the Nuroil trade desk, Sharjah

NURPROOF elastomeric SBS coating
On this page · 6 sections
  1. 01Pinholes
  2. 02Blisters
  3. 03Wash-off and soft film
  4. 04Thin areas and cracking
  5. 05Poor adhesion
  6. 06Preventing defects starts with the right product and documents

Liquid-applied elastomeric SBS bitumen coatings are forgiving to apply: brush, roller or spray, no torches, and they follow awkward shapes easily. That ease hides a weakness. The coating forms its waterproof film on site, so weather, substrate and technique all affect the result. Most defects fall into a handful of patterns that are easy to recognise and avoid.

Pinholes

Pinholes are tiny holes through the film that let water pass. They come from air escaping from porous concrete as the coating dries, from bubbles whipped into the product by over-vigorous mixing, or from a first coat applied too thickly so its surface skins before air escapes.

  • Prime porous concrete with a diluted coat or the recommended primer to seal pores.
  • Stir slowly to avoid drawing in air.
  • Apply in at least two coats, the second at right angles to the first, so any pinholes in one coat are covered by the next.

Blisters

Blisters are bubbles between the coating and the substrate, or between coats. Moisture in the concrete that turns to vapour in sun is the usual cause, along with applying a second coat before the first is dry and trapping water beneath it. Coating hot surfaces in direct sun also increases the risk.

  • Check that slabs are cured and surface dry; water-based coatings tolerate slight dampness but not standing water.
  • Let each coat dry fully before the next; data sheets state minimum recoat times.
  • In hot climates, coat in the cooler part of the day.

Wash-off and soft film

A water-based coating that has not yet dried can be re-emulsified and washed off by rain or dew. Product data sheets commonly advise against outdoor application when rain is expected in the following day or two. In cool or humid weather, drying slows considerably, and the film may stay soft longer than expected.

  • Check the forecast and protect fresh work.
  • Do not apply below the minimum temperature on the data sheet, and never when frost is possible.
  • Do not backfill or cover until the film is fully cured.

Thin areas and cracking

A coating that splits over cracks or wears through has usually been applied too thin. Thickness falls away on edges, high spots and vertical faces, and when the product has been over-diluted. Guidance on liquid membranes stresses specifying and checking the dry film thickness rather than only the quantity used.

  • Check wet film thickness with a comb gauge during each coat.
  • Reinforce corners, cracks and joints with a polyester or glass fabric embedded in the first coat.
  • Do not dilute beyond what the data sheet allows for priming.

Poor adhesion

Peeling usually means dust, laitance, release agents or oil on the substrate, or a surface that was too wet. Old coatings may also be incompatible. Wire-brush or grind weak surfaces, remove dust, and test adhesion on a small area before coating a large old surface.

DefectMain causeFix
PinholesAir from porous concrete; mixing bubblesPrime; two coats at right angles
BlistersTrapped moisture; early recoatCut out, dry, patch and recoat
Wash-offRain before dryingRemove soft material, recoat when dry
Splits over cracksFilm too thin; no reinforcementAdd fabric and extra coat
PeelingDirty or weak substrateRemove, prepare surface, recoat

Preventing defects starts with the right product and documents

Ask for the data sheet with drying times, recoat intervals, minimum application temperature and recommended dry film thickness, and keep it on site. Check batch numbers and shelf life on arrival, since aged or frozen emulsions may not form a proper film. Nuroil supplies elastomeric SBS bitumen coating with a certificate of analysis and safety data sheet; use request a quote or contact us with your project details.

PRODUCTS IN THIS ARTICLE
KEEP READING

More from the Knowledge Centre.

STILL HAVE A QUESTION?

Ask the people who trade it every day.

Our trade managers answer technical and commercial questions about grades, specifications, packing and shipping.

LET’S TALK ABOUT YOUR REQUIREMENTS

Your next shipment starts here.

Request a quote