Technical document

· PDF

Tell us who you are and the document downloads straight away. We use these details only to follow up on your requirement.

Samples & documents

What can we send you?

Tick what you need
Request a quote
Guide3 min read8 sections

Knowledge centre · Waterproofing & construction

Reading an HPMC specification sheet for construction grades

What each line on an HPMC technical data sheet or certificate means, from viscosity and moisture to gel temperature, particle size and surface treatment.

Written by the Nuroil trade desk, Sharjah

Pencil sketch of a roof being waterproofed with bitumen membrane
On this page · 8 sections
  1. 01Identity and composition
  2. 02Viscosity
  3. 03Moisture and ash
  4. 04Physical properties
  5. 05Gel temperature
  6. 06Surface treatment
  7. 07Lot certificate versus data sheet
  8. 08Building your purchase specification

A technical data sheet or certificate of analysis for construction-grade HPMC lists a dozen or so parameters. Some are about identity and purity, some predict how the product will behave in a mortar, and some are mainly useful for incoming quality control. This guide goes through the usual entries and explains what to look for.

Identity and composition

  • Product type: confirms the material is hydroxypropyl methylcellulose and not another cellulose ether such as hydroxyethyl methylcellulose (HEMC) or methylcellulose. These behave similarly but are not identical, particularly in gel temperature.
  • Methoxyl content and hydroxypropoxyl content: the degree of substitution, given as percentages. These influence solubility, gel temperature and surface activity. Pharmacopoeias classify hypromellose into types such as 2910, 2906 and 2208, where the digits indicate approximate methoxyl and hydroxypropoxyl percentages; construction grades may fall within or outside these types.

Viscosity

The most important line. Check that it states the concentration (usually 2%), temperature (often 20 °C), instrument (Brookfield or NDJ), and ideally spindle and speed. Data sheets quote a range; certificates quote a measured value for the lot. Brookfield and NDJ figures differ substantially for the same material, so never compare grades measured on different methods. Pharmacopoeias allow 75% to 140% of the labelled value for higher-viscosity hypromellose; construction suppliers set their own ranges.

Moisture and ash

  • Moisture (loss on drying): measured by drying at 105 °C. Pharmacopoeial hypromellose is limited to 5.0%. Higher moisture means less active product per kilogram and a greater risk of caking.
  • Ash (residue on ignition or sulphated ash): mainly salts left from manufacture. Pharmacopoeial grades are limited to 1.5%; construction grades are often allowed more. A rising ash content between lots can indicate a change in purification.

Physical properties

ParameterWhat it tells you
AppearanceWhite to off-white free-flowing powder; discoloration or lumps suggest a problem
Particle size (e.g. % passing a stated sieve)Finer powder dissolves and thickens faster in the mixer
Bulk densityAffects dosing by volume, silo sizing and bag weight
pH of solutionIndicates residual treatment chemicals; usually near neutral
Gel temperatureTemperature at which a solution gels and loses thickening; higher values tolerate hot conditions better
Surface treatment / dissolution timeWhether the grade disperses without lumps and how quickly it dissolves

Gel temperature

HPMC solutions gel reversibly on heating. Above the gel temperature the polymer comes out of solution and its thickening and water retention fall sharply. For mortars used on hot walls or in hot climates, the gel temperature on the data sheet is worth checking alongside viscosity. It depends on substitution as well as concentration, so compare values measured under the same conditions.

Surface treatment

Many construction grades are surface treated, often by a light crosslinking step, so the powder disperses in water before swelling and then dissolves after a delay. This prevents lumps when a solution is made, and the delay is usually released by alkaline conditions such as a cement mix. Data sheets may show this as "surface treated", "delayed solubility" or a dissolution time. Check that the treatment suits your binder; near-neutral gypsum systems may call for a different grade.

Lot certificate versus data sheet

The technical data sheet gives typical values and ranges for the grade. The certificate of analysis reports actual results for a specific lot. For incoming control, compare each certificate with your agreed specification and keep retained samples. Spot-check viscosity and moisture in your own laboratory using the supplier's method.

Agree the viscosity method, the acceptable range, moisture and particle size in writing before the first order.

Building your purchase specification

Turn the parameters that matter for your product into a short purchase specification: viscosity with method and range, moisture, ash, particle size, surface treatment and gel temperature if relevant, plus packing, labelling and the documents required. Nuroil supplies HPMC on request for construction chemical manufacturers with a CoA on every delivery and the SDS on request; send your specification through the quote form.

PRODUCTS IN THIS GUIDE
KEEP READING

More from the Knowledge Centre.

STILL HAVE A QUESTION?

Ask the people who trade it every day.

Our trade managers answer technical and commercial questions about grades, specifications, packing and shipping.

LET’S TALK ABOUT YOUR REQUIREMENTS

Your next shipment starts here.

Request a quote