Buyers frequently receive tenders written in one grading system while suppliers quote in another. A road authority may specify VG-30, a contractor may ask for 60/70, and an offer may arrive as AC-30. This guide gives the approximate correspondence between the systems and explains why it is only approximate.
Why there is no exact conversion
Each system measures a different property. Penetration grading uses a needle test at 25°C. Viscosity grading uses absolute viscosity at 60°C. Two binders with the same penetration can have different viscosities at 60°C, because bitumens from different crudes and refining routes change stiffness with temperature at different rates. So a 60/70 binder may fall into VG-30 or, occasionally, outside it.
That is also why viscosity grading was introduced: to control the property most closely tied to hot-weather performance rather than inferring it from a room-temperature test.
Approximate correspondence
The table below combines the replacements described by Indian refiners when IS 73 moved from penetration to viscosity grades, and the published 60°C bands of IS 73 and ASTM D3381.
| VG grade (IS 73) | 60°C viscosity, poise | Closest AC grade | Older penetration grade it replaced | Penetration at 25°C, min under IS 73 |
|---|---|---|---|---|
| VG-10 | 800–1200 | AC-10 | 80/100 | 80 |
| VG-20 | 1600–2400 | AC-20 | None directly | 60 |
| VG-30 | 2400–3600 | AC-30 | 60/70 | 45 |
| VG-40 | 3200–4800 | AC-40 | 30/40 | 35 |
Notes on the table:
- Each VG grade shares its 60°C band with the AC grade of the same number, but the two standards are not interchangeable.
- Other limits (flash point, 135°C viscosity, ageing tests) differ between IS 73 and ASTM D3381.
- VG-40 is sometimes loosely compared with 40/50. Indian refiners describe it as replacing the old, harder 30/40 grade.
Which grade for which climate
IS 73 links each viscosity grade to the seven-day average maximum air temperature over the design period, which gives a useful way to think about all three systems:
| 7-day average max air temperature | VG grade | Typical penetration counterpart |
|---|---|---|
| Below 30°C | VG-10 | 80/100 or softer |
| 30–38°C | VG-20 | Between 80/100 and 60/70 |
| 38–45°C | VG-30 | 60/70 |
| Above 45°C | VG-40 | 40/50 or 30/40 |
Climate is only one input. Traffic volume, loading speed and the layer in the pavement also shift the choice, which is why a hot-region project may still use VG-30 on open carriageway and VG-40 only at junctions and climbing lanes.
Handling a mixed specification
- Find the governing document. The contract specification decides; a grade named in a cover letter does not override it.
- Certify to that system. If the specification says VG-30 to IS 73, the CoA should report IS 73 tests, not just penetration.
- Ask for dual testing when needed. Where a project accepts either system, a certificate showing both 60°C viscosity and penetration with softening point lets the engineer judge the binder directly.
- Check the actual values. A lot near the top of VG-30 behaves differently from one near the bottom; compare numbers, not labels.
- Get approval in writing before substituting one system for another.
Use a cross-reference to shortlist products, never to certify them.
Performance grades
Some tenders now name performance grades such as PG 64-22 or PG 70-10 instead of either system. These are set from the expected high and low pavement temperatures and include tests on aged binder, so they do not map neatly onto VG or penetration grades either. A conventional VG-30 or 60/70 binder may meet a particular PG grade, but that can only be confirmed by running the PG tests on the actual product.
Enquiry checklist
Quote the grade and standard exactly as specified, state whether an alternative system is acceptable, and request a CoA covering the governing standard's full table. Nuroil supplies both viscosity grade and penetration grade bitumen and can match offers to the standard your tender names. Send your specification via request a quote.