Nitric acid in stainless steel pickling and passivation

How nitric acid is used to pickle and passivate stainless steel, how the two processes differ, and what the bath chemistry and acid quality involve.

Written by the Nuroil trade desk, Sharjah

On this page · 5 sections
  1. 01Pickling and passivation are different jobs
  2. 02Typical nitric passivation conditions
  3. 03Making up and running a bath
  4. 04Hazards specific to these processes
  5. 05Acid quality for metal finishing

Stainless steel resists corrosion because of a very thin, chromium-rich oxide film on its surface. Fabrication damages that film. Welding leaves heat tint and scale, grinding and machining leave embedded iron particles, and handling with carbon steel tools contaminates the surface. Nitric acid is central to the two treatments used to restore it: pickling and passivation.

Pickling and passivation are different jobs

01

Pickling

removes metal. It strips away weld scale, heat tint and the chromium-depleted layer just beneath it, taking off a thin layer of the steel surface. For stainless steel, the traditional pickling bath is a mixture of nitric acid and hydrofluoric acid. The hydrofluoric acid does most of the dissolving of oxide, and the nitric acid keeps the bath oxidising, controls attack on the base metal and helps the surface repassivate.
02

Passivation

removes little or no base metal. It dissolves free iron and other contaminants from the surface and allows a uniform chromium oxide film to form. Nitric acid alone is a classic passivating agent because it is strongly oxidising but, at the right strength, does not attack stainless steel significantly.

A heavily welded fabrication may need pickling followed by passivation. A clean machined part may only need passivation.

Typical nitric passivation conditions

The widely used specification for passivating stainless steel parts, ASTM A967, describes several nitric acid treatments. Published summaries list baths ranging from about 20 to 55% nitric acid by volume, operated from room temperature up to roughly 55 to 60 °C, for at least 20 to 30 minutes depending on the method. Some methods add sodium dichromate, and one general method allows other combinations provided the treated parts pass the specified tests.

The methods are not interchangeable. Different stainless steel families, such as standard austenitic grades, free-machining grades and martensitic grades, respond differently, and a bath that suits one can etch another. Users should select the method from the current standard and the customer's specification, then verify results with the required test, such as water immersion, humidity, salt spray or a copper sulphate test.

Making up and running a bath

  • Baths are usually made up from 55 to 68% industrial nitric acid diluted with clean water. Always add acid to water, slowly and with mixing, never the reverse.
  • Water quality matters. Chloride in make-up water can cause pitting of stainless steel, so low-chloride or deionised water is preferred.
  • Bath strength falls and dissolved metal rises with use. Regular titration and records of dissolved iron help decide when to top up or replace the bath.
  • Thorough rinsing after treatment, often ending with clean or deionised water, prevents acid residues and staining.

Hazards specific to these processes

Nitric acid baths give off acid mist and, when they react with metal or scale, nitrogen oxides, which are toxic and can cause delayed lung injury. Tanks need local exhaust ventilation and fume scrubbing. Mixed nitric and hydrofluoric pickling adds the severe hazards of hydrofluoric acid, which penetrates skin and requires specific first aid; sites using it must have calcium gluconate gel and trained staff available. Spent pickle liquor contains acids and dissolved metals and must be neutralised and treated before disposal under local rules.

Pickling removes a layer of metal; passivation cleans the surface so the protective oxide can form. Nitric acid does both jobs, at different strengths and with different partners.

Acid quality for metal finishing

Finishing shops usually specify concentration, low chloride content and low iron content. Chloride is the main concern because it undermines the very passive film the process is meant to create. When enquiring, state the concentration, packing (drums, IBCs or bulk), monthly volume and any impurity limits from your process specification. Nuroil provides a CoA with every delivery and the SDS on request. Use the quote request form to share your requirements.

KEEP READING

More from the Knowledge Centre.

STILL HAVE A QUESTION?

Ask the people who trade it every day.

Our trade managers answer technical and commercial questions about grades, specifications, packing and shipping.

LET’S TALK ABOUT YOUR REQUIREMENTS

Your next shipment starts here.

Request a quote