Reading a test certificate for AS 2008 bitumen

A line-by-line guide to the certificate of analysis for AS 2008 bitumen: tests, methods, units and the common points that buyers misread.

Written by the Nuroil trade desk, Sharjah

Pencil sketch of Australian multigrade bitumen
On this page · 7 sections
  1. 01Header information
  2. 02The test lines and what they mean
  3. 03Units and decimal places
  4. 04Original or aged: the most common misreading
  5. 05The durability test in context
  6. 06Red flags
  7. 07Documents to ask for with AS 2008 bitumen

A certificate of analysis is the buyer's main evidence that a bitumen cargo meets AS 2008. It lists each test, the method, the result and the specification limit. Reading it carefully before accepting a shipment can avoid disputes later. This guide walks through the lines you are likely to see and what to check on each.

Header information

Before looking at results, confirm the basics:

  • Product name and class, written exactly as in the contract, for example Class 320 or M500.
  • The standard and its edition, since limits can change between editions.
  • Batch, tank or lot number, and sampling date and point.
  • Name of the laboratory, and whether it is the producer's laboratory or an independent one.

The test lines and what they mean

TestMethod seriesWhat it tells youWhat to check
Viscosity at 60°CAS 2341.2Sets the classInside the class band, on the correct basis (original or aged)
Viscosity at 135°CAS 2341.2Handling at mixing and spraying temperaturesWithin the limit for the class
Penetration at 25°CAS 2341.12Consistency at moderate temperatureMeets the minimum for the class
Flash pointAS 2341.14Fire safety marginAbove the minimum
RTFO residue viscosityAS 2341.2 on residueHardening in the asphalt plantRatio to original within limit, or band for Class 450 and M1000
Durability (sealing binders)AS/NZS 2341.13Resistance to long-term ageing in thin filmsResult reported where the class or contract requires it

Some certificates also show matter insoluble in toluene, which checks for contamination, and density, which is needed to convert between volume and mass.

Units and decimal places

Viscosity at 60°C is reported in pascal-seconds. Older documents or overseas laboratories may use poise, where 10 poise equals 1 Pa·s. Penetration is in tenths of a millimetre, written as dmm or 0.1 mm. Check units carefully before comparing figures with the limit, as a unit error can make a compliant result look out of specification or the reverse.

Original or aged: the most common misreading

For most classes the 60°C band applies to the bitumen as supplied. For Class 450 and M1000 it applies to the residue after the rolling thin film oven test. A certificate should state the basis clearly. If it does not, ask for clarification before accepting the cargo.

The durability test in context

Australia has long used a durability test to judge how quickly an unmodified sealing binder hardens in a thin film exposed to heat and air. The test relies on specialised equipment and is being reviewed, with research looking at pressure ageing and dynamic shear rheometer methods as possible replacements. If your contract calls for a durability result, confirm early that the chosen laboratory can run it, as capacity can be limited.

If any result is borderline, ask whether a retained sample from the same batch can be retested by an independent laboratory before loading, rather than after arrival when options are limited.

Red flags

  • Results that sit exactly on a limit for several tests, with no decimals reported.
  • A certificate dated well before loading with no explanation of tank history.
  • Missing residue tests where the class or contract requires them.
  • A batch number that does not match the bill of lading or tank records.
Check the class, the basis, the units and the batch before you check the numbers.

Documents to ask for with AS 2008 bitumen

Ask for the certificate of analysis for the actual loaded batch, the product safety data sheet, and, where needed, a certificate of origin and an independent inspection report covering quantity and quality at loading. Agree in advance who keeps retained samples and for how long. Nuroil provides a certificate of analysis with every delivery and can arrange the other documents on request through the quote request form.

PRODUCTS IN THIS GUIDE
KEEP READING

More from the knowledge centre.

STILL HAVE A QUESTION?

Ask the people who trade it every day.

Our trade managers answer technical and commercial questions about grades, specifications, packing and shipping.

LET’S TALK ABOUT YOUR REQUIREMENTS

Your next shipment starts here.

Request a quote